pr-w-1102.21-4012-002 rev 0 welding procedure specification for steel structure (wps)-sw(1)
TRANSCRIPT
![Page 1: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/1.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 1/10
PTT PUBLIC COMPANY LIMITED RATCHABURI WORLD COGENERATIONCOMPANY LIMITED
GAS PIPELINE AND GAS METERING AND REGULATING STATION PROJECT
DOCUMENT TITLE: WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS)
DOCUMENT NO.: PR-W-1102.21-4012-002 REVISION: 0
REVIEW STAMP COMMENTS
E. Work may proceed.
F. Work may proceed. Submit “for Construction”
Documents.
G. Revise and Resubmit. Work may proceedSubject to incorporation of changes indicated.
H. Revise and Resubmit. Work may not proceed.
I. Review not required. Work may proceed.
Acceptance in any of these categories shall be in no wayrelieve the Contractor/Supplier of its responsibility for thedue and proper performance of the Work in accordancewith the Contract/Purchase Order.
Name:
Sign:
Date:
0 02/04/13 Issued for Construction WS JR NP
A 05/02/13 Issued for Approval WS JR NP
Rev. Date DescriptionPrepared
ByChecked
By Approved
By
CONTRACTOR:
SIAM RAJATHANEE JOINT VENTURE
CONSULTANT:
UNITY ENGINEERING AND CONSULTANCY
SERVICES CO.,LTD.
![Page 2: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/2.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 2/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 2 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
DOCUMENT CHANGE RECORD
Rev Date Prepared/
Revised
By
ReviewedBy
ApprovedBy
Description
A 05-02-2013 WS JR NP Issued for Approval
0 02/04/13 WS JR NP Issued for Construction
![Page 3: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/3.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 3/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 3 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
TABLE OF CONTENTS
ARTICLE PAGE
1.0 SCOPE ...................................................................................................................................... 4
2.0 REFERENCE ............................................................................................................................. 4
3.0 DEFINITIONS ............................................................................................................................ 4
4.0 VENDOR DOCUMENT .............................................................................................................. 8
![Page 4: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/4.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 4/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 4 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
1.0 SCOPEThis Procedure is for the Welding of Gas Pipeline and Gas Metering and Regulating Station Project.The Material of Pipe used is under standard of ASTM A36, ASTM A53 for Structural Steel. Theapplied Welding Procedure are SMAW for Steel Structure
2.0 REFERENCE
ASTM A36 Standard Specification for Carbon Structural Steel
ASTM A35 Specification for Pipe, Steel, Black and Hot-Dipped Zinc-Coated Welding and Seamless Pipe
AWS D1.1 Structural Welding Code
SP-S-1102.21-010-001 Specification for Civil/Structural Furnishing of StructuralSteel, Miscellaneous Steel & Joint
SP-S-1102.21-010-002 Specification for Civil/Structural Erection of Structural Steel,Miscellaneous Steel & Joints
3.0 DEFINITIONS
WPS Welding Procedure Specification
PQR Procedure Qualification Record
![Page 5: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/5.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 5/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 5 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS)
Welding Process (es) _______________ SMAW______________
Supporting PQR No. (s)_______________-__________________
Joint Design ______________________ Butt W eld____________
Application Code (s) ______________ AWS D1.1_____________
Specification (s)________SP-W- MOC08/2012-504-002________
Identification__________________________________________
Revision_____A___Date___xx/xx/xxx______By______________
Authorized by___________________Date____xx/xx/xxxx______
Type – Manual ( / ) Semi – Automatic ( )
Machine ( ) Automatic ( )
JOINT DESIGN USED
Type_______________Square Groove Weld_________________
Single ( / ) Double Weld ( )
Backing Yes ( ) No ( / )
Backing Material______________ _N/A_____________________
Boot Opening____T1/2__Root Face Dimension_____N/A_______
Groove Angle____N/A__Radius (J-U) __________N/A_________
Back Gouging: Yes ( / ) No ( )
Method____________________Grinding____________________
POSITION
Position of groove________________ALL___________________
Vertical Progression : Up ( / ) Down ( )
ELECTRICAL CHARACTERISTIC
Transfer Mode (GMAW) Short – Circuiting ( )
Grobular ( ) Spray ( )
Current : AC ( / ) DCEP ( ) DCEN ( ) PULSED ( )
Other
BASE METALS
Material Spec.______________ASTM______________________
Type or Grade___________A36 or Equivalent __ _______
Thickness Groove ____T≤ 6.4 mm___ Fillet______YES_________
Diameter (Pipe) _________________N/A ___ ________________
TECHIQUE
Stringer or Weave Bead______________Both________________
Multi – pass or Single Pass (per side)________Both___________
Number of electrodes ________________Single______________
Electrode Spacing Longitudinal ___________N/A__________
Lateral ______ ____N/A_________
Angle_ __________N/A_________
NDT
VISUAL :_________________100%_______________________
DPI :____________________100%_______________________
FILLTER METALS
AWS Specification ________ ________AWS 5.1______________
AWS Classification ___ E7016 and E7018 for Field Welding_____
Type and Brand Name __E7016 (KOBE LB-52 or EQUIVALENT)_
_ E7018 (KOBE LB-52 or EQUIVALENT)_
SHIELDING
Flux_____________N/A________Gas________N/A___________
Composition______N/A_______
Electrode – Flux (Class) Flow Rate________N/A_______
Gas Cup Size_____N/A_______
Contract Tube to Work Distance____________N/A____________
Peening__________________________N/A_________________
Interpass Cleaning: _________ __Grinding – Power Brush______
PREHEAT
Preheat Temp., Min._______________N/A__________________
Interpass Temp.,Min.______________N/A___________________
POSTWELD HEAT TREATMENT
Temp.____________________N/A________________________
Temp.____________________N/A________________________
WELDING PROCEDURE
Passor
WeldLayer
(s)
Process
Filler Metals Current
VoltsTravelSpeed
(cm/min)
Joint Details
Class Diam.Type &Polarity
Amps or WireFeed Speed
ROOT SMAW E7016 3.2 mm AC 80 – 140 22 - 28 5 – 10
H.P SMAW E7016 3.2 mm AC 80 – 140 22 – 28 5 – 10
FILLER SMAW E7016 4.0 mm AC 110 – 190 22 – 28 5 – 10
CAP SMAW E7016 4.0 mm AC 110 - 190 22 - 28 5 – 10
![Page 6: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/6.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 6/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 6 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS)
Welding Process (es) _______________ SMAW______________
Supporting PQR No. (s)_______________-__________________
Joint Design _____________Complete Joint Penetration _______
Application Code (s) ______________ AWS D1.1_____________
Specification (s)_________ SP-W- MOC08/2012-504-002_______
Identification__________________________________________
Revision_____A___Date___xx/xx/xxx______By______________
Authorized by___________________Date____xx/xx/xxxx______
Type – Manual ( / ) Semi – Automatic ( )
Machine ( ) Automatic ( )
JOINT DESIGN USED
Type_______________Square Groove Weld_________________
Single ( / ) Double Weld ( )
Backing Yes ( ) No ( / )
Backing Material______________ _N/A_____________________
Boot Opening_0 – 3 MM__Root Face Dimension___0 – 3 MM_____
Groove Angle ___60 ̊__Radius (J-U) __________N/A_________
Back Gouging: Yes ( / ) No ( )
Method____________________Grinding____________________
POSITION
Position of groove________________1G – 3G___________________
Vertical Progression : Up ( / ) Down ( )
ELECTRICAL CHARACTERISTIC
Transfer Mode (GMAW) Short – Circuiting ( )
Grobular ( ) Spray ( )
Current : AC ( / ) DCEP ( ) DCEN ( ) PULSED ( )
Other
BASE METALS
Material Spec.______________ASTM______________________
Type or Grade_________ _ A36 or Equivalent ______________
Thickness Groove __6.4 < T ≤ 19 mm _Fillet_____N/A_________
Diameter (Pipe) _______________________ ________________
TECHIQUE
Stringer or Weave Bead______________Both________________
Multi – pass or Single Pass (per side)________Both___________
Number of electrodes ________________Single______________
Electrode Spacing Longitudinal ___________N/A__________
Lateral ______ ____N/A_________
Angle_ __________N/A_________
NDT
VISUAL :_________________100%_______________________
DPI :____________________100%_______________________
FILLTER METALS
AWS Specification ________ ________AWS 5.1______________
AWS Classification ___ E7016 and E7018 for Field Welding_____
Type and Brand Name __E7016 (KOBE LB-52 or EQUIVALENT)_
_ E7018 (KOBE LB-52 or EQUIVALENT)_
SHIELDING
Flux_____________N/A________Gas________N/A___________
Composition______N/A_______
Electrode – Flux (Class) Flow Rate________N/A_______
Gas Cup Size_____N/A_______
Contract Tube to Work Distance____________N/A____________
Peening__________________________N/A_________________
Interpass Cleaning: _________ __Grinding – Power Brush______
PREHEAT
Preheat Temp., Min._______________N/A__________________
Interpass Temp.,Min.______________N/A___________________
POSTWELD HEAT TREATMENT
Temp.____________________N/A________________________
Temp.____________________N/A________________________
WELDING PROCEDURE
Passor
WeldLayer
(s)
Process
Filler Metals Current
VoltsTravelSpeed
(cm/min)
Joint Details
Class Diam.Type &Polarity
Amps or WireFeed Speed
ROOT SMAW E7016 3.2 mm AC 80 – 140 22 - 28 5 – 10
H.P SMAW E7016 3.2 mm AC 80 – 140 22 – 28 5 – 10
FILLER SMAW E7016 4.0 mm AC 110 – 190 22 – 28 5 – 10
CAP SMAW E7016 4.0 mm AC 110 - 190 22 - 28 5 – 10
![Page 7: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/7.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 7/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 7 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
}
WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS)
Welding Process (es) _______________ SMAW______________
Supporting PQR No. (s)_______________-__________________
Joint Design ______________________ Fillet Weld___________
Application Code (s) ______________ AWS D1.1_____________
Specification (s)_________ SP-W- MOC08/2012-504-002_______
Identification__________________________________________
Revision_____A___Date___xx/xx/xxx______By______________
Authorized by___________________Date____xx/xx/xxxx______
Type – Manual ( / ) Semi – Automatic ( )
Machine ( ) Automatic ( )
JOINT DESIGN USED
Type_______________Fillet Weld_______ __________
Single ( / ) Double Weld ( )
Backing Yes ( ) No ( / )
Backing Material______________ _N/A_____________________
Boot Opening____0__Root Face Dimension_____ T ≤ 20 MM ____
Groove Angle____N/A__Radius (J-U) __________N/A_________
Back Gouging: Yes ( ) No ( / )
Method____________________Grinding____________________
POSITION
Position of groove________________ALL___________________
Vertical Progression : Up ( / ) Down ( )
ELECTRICAL CHARACTERISTIC
Transfer Mode (GMAW) Short – Circuiting ( )
Grobular ( ) Spray ( )
Current : AC ( / ) DCEP ( ) DCEN ( ) PULSED ( )
Other
BASE METALS
Material Spec.______________ASTM______________________
Type or Grade__________ A36 or Equivalent __ ____________
Thickness Groove ____N/A ___Fillet______N/A _________
Diameter (Pipe) _______________________ ________________
TECHIQUE
Stringer or Weave Bead______________Both________________
Multi – pass or Single Pass (per side)________Both___________
Number of electrodes ________________Single______________
Electrode Spacing Longitudinal ___________N/A__________
Lateral ______ ____N/A_________
Angle_ __________N/A_________
NDT
VISUAL :_________________100%_______________________
DPI :____________________100%_______________________
FILLTER METALS
AWS Specification ________ ________AWS 5.1________________
AWS Classification ___ E7016 and E7018 for Field Welding_____
Type and Brand Name __E7016 (KOBE LB-52 or EQUIVALENT)_
_ E7018 (KOBE LB-52-18 or EQUIVALENT)_
SHIELDING
Flux_____________N/A________Gas________N/A___________
Composition______N/A_______
Electrode – Flux (Class) Flow Rate________N/A_______
N/A Gas Cup Size_____N/A_______
Contract Tube to Work Distance____________N/A____________
Peening__________________________N/A_________________
Interpass Cleaning: _________ __Grinding – Power Brush______
PREHEAT
Preheat Temp., Min._______________N/A__________________
Interpass Temp.,Min.______________N/A___________________
POSTWELD HEAT TREATMENT
Temp.____________________N/A________________________
Temp.____________________N/A________________________
WELDING PROCEDURE
Passor
WeldLayer
(s)
Process
Filler Metals Current
VoltsTravelSpeed
(cm/min)
Joint Details
Class Diam.Type &Polarity
Amps or WireFeed Speed
1 SMAW E7016 3.2 mm AC 90 – 140 20 – 28 5 – 20
SMAW E7016 4.0 mm AC 130 – 190 20 – 28 5 – 20Base Metal Thickness Minimum Size OF Fillet Weld
SMAW E7016 4.0 mm AC 150 - 240 20 - 28 5 – 20
T < 6.4 3 mm.(Single-passweld must be
used)6.4 < T < 12.7 5 mm.
12.7 < T < 20.0 6 mm
![Page 8: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/8.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 8/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 8 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
4.0 VENDOR DOCUMENT- KOBELCO LB – 52 E7016
- KOBELCO LB – 52 – 18 E7018
![Page 9: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/9.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 9/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 9 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))
![Page 10: Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)](https://reader037.vdocuments.us/reader037/viewer/2022100404/577cd2e61a28ab9e78964370/html5/thumbnails/10.jpg)
8/13/2019 Pr-w-1102.21-4012-002 Rev 0 Welding Procedure Specification for Steel Structure (Wps)-Sw(1)
http://slidepdf.com/reader/full/pr-w-110221-4012-002-rev-0-welding-procedure-specification-for-steel-structure 10/10
WELDING PROCEDURESPECIFICATION FOR STEEL
STRUCTURE (WPS)
GAS PIPELINE AND GAS METERING ANDREGULATING STATION PROJECT
Document No. PR-W-1102.21-4012-002
Rev. 0 Page 10 of 10
PR-W-1102.21-4012-002 Rev.0(WELDING PROCEDURE SPECIFICATION FOR STEEL STRUCTURE (WPS))