NISTM ~ Ohio Storage Tank Conference Storage Tank Welding

Upload: others

Post on 21-Feb-2020

76 views

Category:

Documents


6 download

TRANSCRIPT

Page 1: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

NISTM ~ Ohio Storage Tank

Conference

Storage Tank Welding

Page 2: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Modern Welding Company

• Welding Fabricator since 1932

– Storage Tanks

– Pressure Vessels

– Structural Steel

• Presented by:

• Phil Grimm

Page 3: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Welding Processes

• SMAW ~ Shielded Metal Arc Welding

• GMAW ~ Gas Metal Arc Welding

• FCAW-G ~ Flux Cored Arc Welding – Gas Shield

• SAW ~ Submerged Arc Welding – Machine

• Filler Metal Tensile Strength Matches Base Metal Tensile Strength

Page 4: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

SMAW Shielded Metal Arc

Welding

• Welder Friendly

• All Positions

• Portable

• Least cost efficient

• Frequent stops

Page 5: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

GMAW-S Gas Metal Arc Welding ~

Short-Circuiting

• High Deposition

Rate

• All Positions

• Continuous

Welding

• Low Penetration

Page 6: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

FCAW-G Flux Corded Arc Welding

~ Gas Shielding

• Slag Supports Weld

Bead

• All Positions

• Continuous Welding

• Good Penetration

Page 7: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

SAW Submerged Arc Welding

• Machine Welding

• Cost Efficient

• High Quality

• Flat Position Only

Page 8: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Machine Welding

• Joggle Joint

• Welding With

Backing

• CP One Side

Page 9: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Properties of a Welded Joint

• Full Penetration

• Complete Fusion

• Filler Metal Compatibility

• Position of Electrode

Page 10: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Welding Process Productivity

Manual and Semi-Automatic

0

2

4

6

8

10

12

14

16

18

20

1/4" 5/16" 3/8" 7/16"

SMAW

GMAW

FCAW

Page 11: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

The WPS should list all

Technical Requirements

• Nozzle Placement

• Position

• Filler Metal

• Base Metal

• Volts & Amps

• Temperature

• Gas ~ if required

• Flux ~ if required

• Electrical Characteristics

• Electrode Direction

Page 12: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

Welding Procedure Qualification

ANSI/AWS B2.1-98 “Specification for

Welding Procedure and Performance

Qualification”

• Standard Welding Procedures

• Pre-Qualified Welding Procedures

• Qualified WPS to B2.1

Page 13: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

AWS D1.1

“Structural Welding Code”

• AWS Pre-qualified

Welding Procedure

Specification in D1.1.

American Welding

Society

Page 14: Storage Tank WeldingWelding Procedure Qualification ANSI/AWS B2.1-98 “Specification for Welding Procedure and Performance Qualification” •Standard Welding Procedures •Pre-Qualified

NISTM ~ Ohio Storage Tank

Conference

Storage Tank Welding