Download - Delcrete
General
Delcrete™ m Elastomeric Concrete is a pour-in-place, free-flowing, two-part polyurethane-based elastomeric concrete. Delcrete™ m has been compounded to bond to a variety of surfaces including steel and concrete. Following are the design features of the industry’s premier elastomeric concrete:
Mixing/Components
Part A - 1500 ML ClearPart B - 3000 ML Black
www.dsbrown.com
The D.S. Brown Company
Product Datasheet
Delcrete™ mD.S. Brown Co.
Founded in 1890 and based in North
Baltimore, Ohio, USA, The D.S. Brown
Company is a worldwide designer, man-
ufacturer and supplier of engineered
products for the highway and bridge
construction markets.
D.S. Brown is fully integrated, perform-
ing and controlling all requirements of
a project internally:
• Research and Development
• Engineering Design/CAD Detailing
• Load Testing
• Rubber Compounding, Mixing,
Extruding and Molding
• Custom Steel Fabrication and
Machining
PROTECT YOUR INVESTMENT
HEADQUARTERS
300 East Cherry
North Baltimore, Ohio 45872
CONTACT
Phone (419) 257-3561
Fax (419) 257-2200
www.dsbrown.com
© 2008 D.S. Brown - All rights reserved.
DSB ML-Delcrete m - Datasheet-01
• Polyurethane chemistry • Non-brittle over extreme temperature ranges • Permanent, long-term repair solution • Resistant to nearly all chemicals • One hour cure time
One 48 lb bag of aggregate. One batch is equal to 3.5 mixed gallons. 12 batches per unit is equal to 42 mixed gallons. 42 gallons is equal to 5.6 cubic feet per unit.
DELCRETE BINDER & AGGREGATE
TEST TEST METHOD SPECIFICATION
Original Properties (after conditioning at 100 F [37 C]
for 7 days)
Tensile Strength, psi (MPa) Note 1 600 (4.14) Min.
Elongation, % Note 1 25 Min.
Hardness, Durometer D ASTM D2240 50 Shore D Max.
Compressive PropertiesCompressive Stress, psi (MPa) 5%
Deflection ASTM D695, Note 2 800 (5.52) Min.
Resilience, % - 5% Deflection Note 3 70 Min.
Impact Properties Ball Drop, ft.-lb. (Joule) @-20 F (-29C) Note 4 >10 (13.56) (no cracks)
Adhesion PropertiesDry Bond Strength to Concrete, psi (kN/m) Note 5 (Dry) 350 (61.30) Min.Wet Bond Strength to Concrete, psi (kN/m) Note 5 250 (43.78) Min.
Gel Time Tex-614-J 5-30 Minutes
DELCRETE BINDER ONLY
TEST TEST METHOD SPECIFICATION
Original Properties (after conditioning at 100 F [37 C]
for 7 days)
Tensile Strength, psi (MPa) ASTM D638 1,500 (10.34) Min.
Tensile Stress, 100% psi (MPa) ASTM D638 500 (3.45) Min.
Elongation, % ASTM D638 150 Min.
Hardness, Durometer A ASTM D2240 92 +/-3 A
Tensile Properties, After Oven Aging (7 days @ 158 F [70
C])
Tensile Strength, psi (MPa) ASTM D573 (D638) 1,500 (10.34) Min.
Tensile Stress, psi (MPa) ASTM D573 (D638) 500 (3.45) Min.
Elongation, % ASTM D573 (D638) 150 Min.
Hardness, Durometer A ASTM D573 (D2240) 92 +/-3 A