presipitation hardening

16
SUPENDI (2613091037) PRECIPITATION HARDENING UNIVERSITAS JENDERAL ACHMAD YANI BANDUNG

Upload: vendi-supendi

Post on 24-Oct-2014

108 views

Category:

Documents


6 download

TRANSCRIPT

Page 1: Presipitation Hardening

SUPENDI (2613091037)

PRECIPITATION HARDENING

UNIVERSITAS JENDERAL ACHMAD YANI

BANDUNG

Page 2: Presipitation Hardening

PENDAHULUANPresipitation Hardening adalah proses pengerasan paduan logam dengan menyebarkan partikel-partikel halus secara merata. dengan proses penuaan (aging) yang sebelumnya telah mengalami proses pelarutan ( solution treatment) dan pencelupan (quenching)

Syarat Presipitation Hardening :•Merupakan Logam paduan•Batas kelarutan padat harus berkurang dengan turunnya temperatur

Page 3: Presipitation Hardening

PENDAHULUAN

Page 4: Presipitation Hardening

PENDAHULUAN

Skematik temperatur tehadap waktu

Page 5: Presipitation Hardening

Pengaruh waktu aging terhadap sifat mekanik

Page 6: Presipitation Hardening

gambar 2.16. Skematik pengaruh temperatur pada presipitat Al-Cu. (a) Garis solvus metastabil dan (b) waktu memulai pembentukan presipitat

Page 7: Presipitation Hardening

MEKANISME PENGUATAN

Interaksi Dislokasi dengan Presipitat

dislokasiPresipitat

Cutting

Page 8: Presipitation Hardening

MEKANISME PENGUATAN

Bowing

dislokasi

Page 9: Presipitation Hardening

Paduan yang bisa dikeraskan dengan proses presipitation hardening

Page 10: Presipitation Hardening

DIAGRAM FASA Al-Cu

Page 11: Presipitation Hardening

Contoh proses precipitation hardening Al-Cu

Page 12: Presipitation Hardening

Schematic depiction of several stages in the formation of the equilibrium precipitate ( ) phase. (a) A supersaturated solid solution. (b) A transition, precipitate phase. (c) The equilibrium u phase, within the α-matrix phase.

Page 13: Presipitation Hardening

The precipitation hardening characteristics of a 2014 aluminum alloy (0.9 wt% Si, 4.4 wt% Cu, 0.8 wt% Mn, 0.5 wt% Mg) at four different aging temperatures: yield strength,

Page 14: Presipitation Hardening

A transmission electron micrograph showing the microstructure of a 7150-T651 aluminum alloy (6.2Zn, 2.3Cu, 2.3Mg, 0.12Zr, the balance Al) that has been precipitation hardened. The light matrix phase in the micrograph is an aluminum solid solution. The majority of the small plate-shaped dark precipitate particles are a transition phase, the remainder being the equilibrium (MgZn2) phase. Note that grain boundaries are “decorated” by some of these particles. (Courtesy of G. H. Narayanan and A. G. Miller, Boeing Commercial Airplane Company.)

Page 15: Presipitation Hardening

DAFTAR PUSTAKA

William D. Callister, Jr. “Materials Science and Engineering 7th” ,

John Wiley & Sons, Inc. 2007.

R. E. Smallman and R. J. Bishop, “Modern Physical Metallurgy

and Materials Engineering 6th” , Butterworth-Heinemann, 1999.

D.A. Porter and K.E.Easterling, “Phase Transformations in

Metals and Alloys 2nd ” chapman & Hall, 1992.

William F.Smith “ Principles of Materials Science and

Engineering 3rd ” McGraw-Hill Inc, 1993.

Page 16: Presipitation Hardening

SEKIAN

Terima kasih

“ Niscaya Allah akan meninggikan orang-orang yang beriman diantaramu dan orang-orang yang diberi ilmu pengetahuan